Factors affecting the opening machine plasticising
Factors affecting the opening machine plasticising
11/09/2024News
1, the lower the roller temperature roller temperature, the better the plasticising effect.
2, the smaller the roll distance, the better the plasticising effect.
3、Time The plasticising time should be less than 20 minutes, and the next piece is parked for 4~8 hours.
4、Capacity
5、Plasticising agent Temperature control at 70~75℃ The raw rubber moulded with plasticising agent has small elastic recovery, which can reduce the shrinkage of rubber.
Advantages and disadvantages of opening machine plasticising Advantages.
A. Good quality of plasticised rubber, even plasticity.
B, change the rubber species is more flexible.
C, construction investment is small, plant requirements are not high
Disadvantages.
A, low production efficiency
B, labour intensity
C, poor hygiene conditions
We use cookies on our website to see how you interact with it. By accepting, you agree to our use of such cookies. privacy policy
Advanced Cookie Settings
Essential Cookies
These cookies enable core functionality such as security, verification of identity and network management. These cookies can’t be disabled.
Enable Marketing Cookies
These cookies are used to track advertising performance, consent to the sending of advertising-related user data to Google, and consent for the website to serve personalized advertising to provide more relevant services.
Enable Functional Cookies
These cookies collect data to remember choices users make to improve and give a more personalised experience.
Enable Analytics Cookies
These cookies help us to understand how visitors interact with our website, discover errors and provide a better overall analytics.